You cut a box file, pop the parts out, and the tabs rattle in their slots. Or the opposite: nothing goes together without a hammer. In almost every case the cause is the same pair of numbers: the kerf of your laser and the real thickness of your sheet. Measure both once, and most fit problems disappear.
What kerf is
Kerf is the width of material the laser removes as it cuts. The beam is not an infinitely thin line: it has a spot size, and the material burns away a little on each side. On hobby machines the full kerf is typically around 0.1 to 0.25 mm on a CO2 laser and closer to 0.08 mm on a diode laser, but it changes with:
- the material and its thickness (thicker sheets usually burn a wider, slightly tapered cut),
- power and speed,
- focus height and lens,
- air assist.
Because the laser follows the center of the drawn line, every part comes out half a kerf smaller on each side, and every hole comes out half a kerf larger. Tabs shrink, slots grow, and the joint goes loose.
Problem number two: your "3 mm" plywood is not 3 mm
Sheet goods are sold by nominal thickness. "3 mm" plywood can measure anywhere from about 2.8 to 3.2 mm, and "1/8 in" sheets vary just as much, even within one pack. If a file was designed for 3.0 mm slots and your sheet measures 3.15 mm, the parts will not go together, whatever the kerf.
So the first rule is simple: measure every new batch of material with calipers, in a few spots, and use that number.
How to measure kerf
Method 1: the square test
- Draw a 20.00 mm square.
- Cut it in the material and settings you will use for the project.
- Measure the square with calipers on both sides.
- Kerf = 20.00 minus the measured size. A square that measures 19.84 mm means a kerf of 0.16 mm.
Measure the hole the square left as well: it should be about the same amount larger than 20 mm.
Method 2: the comb test (best for joints)
- Draw a strip with a row of slots, each one a little wider than the last: for a 3 mm sheet, for example, from 2.8 mm to 3.3 mm in 0.05 mm steps.
- Label each slot with a small engraved number.
- Cut the strip and a few test tabs from the same sheet.
- Push a tab into each slot. The one that holds firmly by friction, without forcing, is your fit.
The comb test measures kerf and thickness together, which is what really matters for a joint.
How to compensate
There are two approaches, and both work.
Adjust the drawing. Offset outer contours outward by half the kerf, and inner contours (holes and slots) inward by half the kerf. In Inkscape, the Offset path effect does this with an exact distance. Design slots at the measured thickness of your sheet, not the nominal one.
Let the software do it. LightBurn has a kerf offset setting in each cut layer: enter half or full kerf as its manual describes, and it shifts the path in the right direction for outsides and insides. Not every laser program offers this, so the drawing method is the universal one.
A useful habit: keep a kerf notebook, one line per material and setting: "3 mm birch ply, 0.15 mm kerf, slot 3.05 mm for friction fit". After a few months you will rarely need to run a test.
Other reasons parts do not fit
- Scale problems. A file imported at the wrong resolution comes out about 75% or 133% of its size. Check one known dimension before cutting the whole job.
- Taper. On thick material the cut is wider at the top than at the bottom. Put the narrower side where the joint matters, or slow down and refocus.
- Warped sheets. A bowed sheet changes focus across the bed and the kerf with it. Hold it flat with pins or weights.
- Double lines. Overlapping duplicate paths cut twice, burn wider and leave scorch marks. Delete duplicates before cutting.
What a good cut file should give you
When you buy laser files, look for designers who state the material thickness each version is made for, ship separate versions for common thicknesses (3 mm, 1/8 in, 6 mm, 1/4 in), say what kerf compensation is already applied, and include a fit-test strip. Those details save more material than any other feature.
Turning fits into sales
Once your joints are reliable, you can make the same box or organizer in batches. To price a batch properly, count material per sheet, machine minutes and fees: our Craft Business Inventory & Profit Tracker works out the cost and profit of every product for you. See also SVG vs DXF vs PDF for laser cutting.